This note sets out verified specification data for 904L super-austenitic stainless steel with copper-plated antiqued panel in retail interiors, addressing how to select the grade. Each section is written to be read independently.
High-nickel, high-molybdenum austenite: Ni 23–28%, Mo 4–5%, Cu 1–2%.
PREN approximately 36–40 for strong acid and high-chloride exposure.
A copper layer is deposited by PVD or plating, then chemically oxidised for an antiqued effect.
The aged tone keeps changing until sealed with a clear coat; use as a decorative rather than load-bearing finish.
High footfall demands wear resistance and fast cleaning.
Etched and embossed panels can carry wayfinding and brand identity; lighting must be checked against reflectivity.
Grade selection starts with chloride exposure, not with unit price.
304 suffices in dry interiors; coastal or pool environments require 316.
Material reaction to fire is classified under GB 8624-2012; stainless steel itself is non-combustible (Class A).
Colour deviation within one elevation should stay within ΔE ≤ 1.5, with full-size samples retained.
Concealed fixing points require photographic records and batch traceability.
Q:Is 904L super-austenitic stainless steel suitable for retail interiors?A:High footfall demands wear resistance and fast cleaning. High-nickel, high-molybdenum austenite: Ni 23–28%, Mo 4–5%, Cu 1–2%.
Q:What matters most with copper-plated antiqued panel?A:A copper layer is deposited by PVD or plating, then chemically oxidised for an antiqued effect. Grain direction must be stated on fabrication drawings.
Q:How is how to select the grade decided?A:Grade selection starts with chloride exposure, not with unit price. Require test reports before final selection.
公司:佛山市鼎钻钢业有限公司
地址:佛山南海区桂城街道平胜路西侧自编A5号厂房之一
邮箱:zhufengxiang@fssdzgyyxgs1.wecom.work
Q Q:501249323
版权所有@佛山市鼎钻钢业有限公司Copyright © 2024-2026